[MR] A question about shields.....

stickjock at comcast.net stickjock at comcast.net
Tue Sep 6 11:55:34 PDT 2005


I can't speak for everyone but the shields I use are .090 thickness T-6 shaped on an english wheel.  As for the edging I use pinch weld molding in place of the heater hose then cover the entire shield with heavy canvas.  It gives the shield a banded edge look.

Miguel Estevan de Cabra
www.spanishpeacock.com 


-------------- Original message -------------- 

> Can anyone on here tell me what guage of aircraft aluminum folks are using to 
> make these single-layer lightweight heater shields that I saw a few of the 
> knights using at Coronation? Also, are they rolling the edges over a couple of 
> times before putting the heater hose padding on? 
> Thanks, 
> 
> Baron Arkein 
> ======================================================================== 
> The Merry Rose Tavern at Cheapside 
> List Info: http://merryrose.atlantia.sca.org/ 
> Submissions: Atlantia at atlantia.sca.org 
> Subscriptions: http://seahorse.atlantia.sca.org/mailman/listinfo/atlantia 


More information about the Atlantia mailing list